AGS MAGIC® MASTER ALLOYS
|
CARAT SILVER ALLOYS |
MAGIC MASTER ALLOY |
METAL COLOUR |
CASTING TEMPER- ATURE °C | FLASK TEMPER- ATURE °C |
QUENCH AFTER CASTING |
SILVER |
4AG |
Silver Wire+Sheet |
970-990°C |
580-640°C |
15-20 Minutes |
SILVER |
5AG |
Silver Casting |
940-990°C |
580-640°C |
15-20 Minutes |
SILVER |
6AG |
Silver Casting |
940-990°C |
580-640°C |
15-20 Minutes |