AGS MAGIC® MASTER ALLOYS
|
CARAT PLATINUM ALLOYS |
MAGIC MASTER ALLOY |
METAL COLOUR |
CASTING TEMPER- ATURE °C | FLASK TEMPER- ATURE °C |
QUENCH AFTER CASTING |
PLATINUM |
PT 9050 |
PT 950 |
1950-2000°C |
650-900°C |
5-10 Minutes |
PLATINUM |
PT 9050 |
PT 900 |
1900-2000°C |
650-900°C |
5-10 Minutes |